Outgassing Data Introduction

Material
Application
Data Ref
CVCM
TML %
Material Data Ref Mfr. TML % CVCM WVR Application Time 1 Temp 1 ATM 1 Time 2 Temp 2 ATM 2 Time 3 Temp 3 ATM 3 Time 4 Temp 4 ATM 4 Year
EM-166 TYPE K RED EPOXY MOLDING CPND GSFC15984 HTR 0.38 0.00 0.16 MOLD CPND 14M 149 PSI 2H 138 AIR 1986
EM-FAB 20-60 TEFLON IMPREG FIBERGLASS GSFC02314 PAL 0.00 0.00 INSULATION 1970
EMA 7037 IRON GSFC05741 SBI 0.34 0.01 DIELECTRIC 1974
EMA 7085 IRON GSFC05743 SBI 0.23 0.00 DIELECTRIC 1974
EMA 8190 IRON GSFC05745 SBI 0.21 0.00 DIELECTRIC 1974
EMC 115-B-1 GLASS/EPOXY GSFC02260 PAC 0.29 0.00 MOLD CPND 1970
EMC 14107-01-445 GLASS FILLED POLYESTER AQUA GSFC15534 ELC 0.23 0.04 0.08 MOLD CPND 1986
EMC 15108-01-446 GLASS FILLED POLYESTER AQUA GSFC15536 ELC 0.19 0.01 0.07 MOLD CPND 1986
EMC 7195-295-5 PHENOLIC DARK GREEN GSFC15538 ELC 1.33 0.00 0.24 MOLD CPND 1986
EMC 90 - BLACK GSFC07214 PAC 0.60 0.01 0.09 POTTING 5M 150 AIR 1975