RM-400 WHITE, THERMAL AND ELECTRICALLY CONDUCTIVE PAINT |
GSFC30319 |
AZT |
0.21 |
0.01 |
0.16 |
PAINT |
24H |
130 |
E-2 |
|
|
|
|
|
|
|
|
|
2007 |
RMBC 18 A/B AS 4/1 BW CLEAR EPOXY |
GSFC07220 |
RVM |
6.85 |
0.01 |
0.14 |
COATING |
1H |
25 |
AIR |
1H |
132 |
AIR |
|
|
|
|
|
|
1975 |
RNC50 RESISTOR COATING PHENOLIC/EPOXY |
GSFC16251 |
IRI |
0.18 |
0.04 |
0.06 |
COATING |
10M |
160 |
AIR |
|
|
|
|
|
|
|
|
|
1987 |
RNF 3000 (HEAT SHRINK PLYOLEFIN TUBING) |
GSFC33511 |
TYO |
1.09 |
0.19 |
0.12 |
WIRE INSULATION |
|
|
|
|
|
|
|
|
|
|
|
|
2012 |
RNF-100 SHRINK TUBING, BLACK |
GSFC33538 |
RCC |
0.51 |
0.06 |
0.04 |
SHRINK TUBING |
|
|
|
|
|
|
|
|
|
|
|
|
2012 |
RNF-150-1-0 HEAT SHRINK TUBING, BLACK, PRE SHRUNK |
GSFC31354 |
TYC |
0.17 |
0.01 |
0.05 |
SHRINK TUBING |
|
|
|
|
|
|
|
|
|
|
|
|
2009 |
RO 4350B CIRCUIT BOARD MATERIAL, IPC-4103/11 |
GSFC31351 |
ROG |
0.11 |
0.00 |
0.02 |
LAMINATE |
|
|
|
|
|
|
|
|
|
|
|
|
2009 |
RO4003 CU CLAD GLASS REINFORCED HYDROCARBON CERAMIC |
GSFC24339 |
ROG |
0.06 |
0.00 |
0.02 |
LAMINATE |
|
|
|
|
|
|
|
|
|
|
|
|
1997 |
ROBLON COMPOSITE ARAMID FIBER |
GSFC32428 |
RBL |
3.23 |
0.00 |
2.67 |
CABLE INSULATION |
|
|
|
|
|
|
|
|
|
|
|
|
2010 |
ROD JANCO HIGH TEMPERATURE - BLUE |
GSFC15900 |
JAN |
0.60 |
0.01 |
0.19 |
INSUL SHIM |
|
|
|
|
|
|
|
|
|
|
|
|
1986 |